Guide
Glitter Ink Screen Printing: Shimmer & Metallic Guide
Champion Inks

Glitter ink screen printing comes down to three things: a screen open enough for the flake, a deposit thick enough to cover the shirt in sparkle, and a cure that reaches all the way through a heavy ink film. Champion’s specs give 25–40 mesh for Glitter Plastisol Ink, 86–125 for metallic and 110–156 for shimmer, and a full cure of 320°F (160°C) for all three. On dark garments, the glitter page recommends a white or colored underbase “for maximum pop.”
Flake, pearl or metallic: what is in each ink
All three are phthalate-free plastisols made for cotton, blends and polyester. What sets them apart is the particle suspended in the ink, and that particle decides the mesh, the stencil and the print order.
- Glitter: polyester flake. Champion Glitter Plastisol is “a ready-to-print, phthalate-free clear base loaded with polyester glitter flake.” The flake is large enough to need an open mesh, and each piece catches light on its own, so the print reads as bold, separate points of sparkle. Champion lists it as best for “Fashion graphics, cheer, dance, school spirit and holiday designs.”
- Metallic: fine metallic flake. Metallic Plastisol Ink is “loaded with fine metallic flake for a brilliant, reflective finish.” Smaller flake lies closer together, so instead of separate sparkles you get “a smooth, mirror-like sheen.” The range covers gold, silver, copper and black, with several golds including 24K Gold and Rose Gold, so it is the place to start when a job calls for gold metallic ink.
- Shimmer: pearlescent pigment. Shimmer Plastisol Ink uses “fine pearlescent pigment for a soft metallic glow.” In the product page’s words: “Pearlescent finish – smooth shimmer without coarse flake.” Think pearl, not mirror.
Glitter ink screen printing: mesh count and screen setup
Mesh is the setting that matters most. Each opening in the screen has to be comfortably larger than the particle passing through it. If it isn’t, the mesh strains the particle out and the print comes up thin and patchy. Here are Champion’s specs side by side.
| Setting | Glitter | Metallic | Shimmer |
|---|---|---|---|
| What’s in it | Polyester glitter flake in a clear base | Fine metallic flake | Fine pearlescent pigment |
| Mesh | 25–40 (open) | 86–125 | 110–156 |
| Squeegee | 60–70 durometer, slow stroke, firm flood | 60–70 durometer, medium pressure | 65–75 durometer, medium pressure |
| Flash | 220–250°F (104–121°C) until dry to the touch | 220–250°F (104–121°C) until dry to the touch | 220–250°F (104–121°C) until dry to the touch |
| Full cure | 320°F (160°C), entire ink film | 320°F (160°C), entire ink film | 320°F (160°C), entire ink film |
| Print order | Last (general practice) | Last (per the spec) | No special order given |
Glitter: open mesh and a thick stencil
The Glitter Plastisol spec is specific: “Open mesh: 25–40 (glitter flake needs a large opening).” That is much coarser than the screens most shops keep for everyday plastisol, so build glitter screens on purpose instead of pulling whatever is on the rack.
Pair the open mesh with a thick stencil. The product page advises: “Use a thick stencil (high-build emulsion or capillary film) for the brightest sparkle.” A thicker stencil holds more ink in each opening, which puts more flake on the shirt and leaves fewer bare spots between flakes.
On press, the spec calls for a “60–70 durometer, slow stroke, firm flood.” A softer blade and an unhurried stroke give the flake time to clear the mesh, and a firm flood fills the screen evenly before each print. Expect a heavier hand than a standard print; that is the trade for real sparkle.
Coarse mesh can’t hold fine detail either. Keep glitter to bold shapes and lettering, and put hairlines and small type in a finer-mesh color in the same design.
Metallic: open mesh for the flake
Metallic flake is finer, so the screen can be finer too, but it still needs room. The Metallic Plastisol spec gives “86–125 (open mesh lets the flake through)” with a 60–70 durometer squeegee at medium pressure. A finer mesh than that can hold flake back and dull the finish.
Shimmer: standard mesh
Shimmer is the easy one. Its product page says it “Prints like regular plastisol – standard mesh, no special tooling,” and lists 110–156 mesh with a 65–75 durometer squeegee at medium pressure. Because the pigment is fine, shimmer holds more detail than glitter and suits designs where you want a soft sheen across the whole graphic.
Glitter, metallic and shimmer on dark garments
Glitter’s base is clear. On a black shirt you see the flake, but you also see dark fabric in every gap between flakes, which makes the print look thinner than it is. Champion’s glitter page says it prints on light and dark garments, and to “print over a white or colored underbase for maximum pop on darks.”
- White underbase: the brightest result, because the gaps between flakes read light.
- Colored underbase: choose a color close to the glitter, such as a gold-toned base under gold glitter. The gaps then read as the same color and the glitter looks denser.
Print the underbase through a finer mesh than the glitter so its edges stay clean, flash it until it is dry to the touch, then print the glitter on top. Choose the white for the fabric: Champion’s white plastisol underbase inks include whites made for 100% cotton, 50/50 blends and 100% polyester. For the underbase technique itself, see How to Use Champion Inks White Plastisol Ink.
Metallic on darks. The metallic spec doesn’t call for an underbase. On dark shirts many printers still lay down a flashed, smooth underbase under metallic ink: it brightens the color and gives the flake a flat surface to lie on, which helps the shine. Printed straight onto a dark shirt, metallic reads more subdued. That is general practice rather than a Champion instruction, so print a sample both ways on the actual garment.
Shimmer on darks. The shimmer spec doesn’t mention an underbase. Champion describes the effect as “Subtle pearl shimmer that moves with the light,” so sample it on the garment color before you quote the job.
Print order and finishing
Stir before every run
Flake is heavier than the base around it, so it sinks in the container between jobs. Both product pages say so: “Stir well before each use – glitter settles,” and “Stir well – metallic flake settles.” Stir from the bottom until the flake is spread evenly. Skip it and the first prints come out flake-poor while the bottom of the container gets overloaded.
Print metallic and glitter last
The metallic spec is direct: “Print last in the sequence and avoid printing over it wet; a hot press or a clear top-coat adds extra shine.” Anything printed on top hides the flake, and printing into wet metallic ink pulls it onto the next screen. Champion’s glitter page doesn’t set an order, but the same logic applies: put glitter at the end of the sequence so nothing covers the sparkle.
Extra shine: a hot press or a clear top-coat
- Hot press. Once the metallic print is cured, a brief press under a release sheet smooths the surface so the flake lies flatter and reflects more light. The spec doesn’t give press settings, so dial in time, temperature and pressure on a sample.
- Clear top-coat. Flash the metallic rather than printing into it wet, then print a clear over it. Champion’s Overprint Clear Gel is a “transparent plastisol topcoat” that “Adds wet-look shine and definition to graphics.” Its page is written for cotton and cotton-blend garments, so sample it before top-coating polyester.
Curing glitter, metallic and shimmer
All three specs give the same targets: flash at 220–250°F (104–121°C) “until dry to the touch,” and a full cure at 320°F (160°C), where the “entire ink film must reach temperature.” The catch with glitter is the deposit. An open mesh and a thick stencil lay down a much heavier film than a standard print, and the bottom of that film, against the fabric, is the last part to get hot.
- Measure the ink film, not the dryer setting. A probe or temperature strips on the print are more trustworthy than an infrared gun here, because shiny glitter and metallic surfaces can throw off infrared readings.
- Add time, not heat. For heavy glitter deposits, slow the belt to lengthen dwell time rather than raising the temperature, which risks scorching the garment and, on polyester, dye migration.
- Stretch-test a cooled print. Cracking or flake coming loose can point to an under-cured film.
- Wash-test before the run. Champion describes its glitter as “Wash-durable – flake is locked into a flexible plastisol film,” and a test wash confirms your cure delivers that.
- Test polyester first. The glitter page lists polyester with the note “test poly for dye migration.”
Custom glitter with Glitter Particles
When a job needs a glitter color or mix that isn’t in the ready-mixed range, the Glitter Plastisol page has the answer: “Need a custom glitter blend? Add Champion Inks® Glitter Particles to clear base.” Glitter Particles are metallic PET flake (“Material: Polyester (PET)”) in a fine .008" particle size, sold by the pound, and listed to “Mix into plastisol or water-based inks for custom glitter screen printing.”
- Weigh the clear base and the flake, and start with a small test batch.
- Mix until the flake is evenly dispersed, with no clumps at the bottom of the container.
- Start from the open-mesh range on the Glitter Plastisol page (25–40) and adjust from the test print.
- Print on the job’s actual garment, cure to the base’s spec and wash-test the sample.
- Record the ratio by weight so the next batch matches.
Champion’s pages don’t give a loading ratio, so build yours by testing. If you aren’t sure which clear base to pair with the flake, ask Champion.
Shop the inks
- Glitter Plastisol Ink: ready-mixed glitter in a clear plastisol base.
- Metallic Plastisol Ink: fine metallic flake in gold, silver, copper and black.
- Shimmer Plastisol Ink: pearlescent shimmer that prints like standard plastisol.
- Glitter Particles: PET glitter flake by the pound for custom blends.
- Overprint Clear Gel: a clear top-coat for extra gloss.
- White plastisol inks for underbases, and more effects in Champion’s specialty plastisol inks.
Glitter, metallic and shimmer each come in Pint, Quart, Gallon and 5 Gallon sizes, so you can sample a pint before committing to a production run. Printing youth cheer, dance or school orders? Each of the three product pages states: “Phthalate-free formulation, made to meet CPSIA lead and phthalate limits for children’s products,” and links its Safety Data Sheet. Children’s product rules cover the finished garment, not just the ink, so confirm what testing or paperwork your customer needs before you print.
Specs in this guide were checked against Champion’s live product pages on November 24, 2026. If the label on your container differs, follow the label.
Frequently asked questions
What mesh count is best for glitter ink?
Go open. Champion’s Glitter Plastisol spec calls for “Open mesh: 25–40 (glitter flake needs a large opening),” with a thick stencil, a 60–70 durometer squeegee, a slow stroke and a firm flood. A finer mesh strains the flake out and leaves a thin, patchy print. For comparison, Champion’s metallic ink runs on 86–125 mesh and its shimmer ink on 110–156.
Do you need an underbase for glitter or metallic ink on black shirts?
For glitter, yes if you want full impact: Champion’s page says to “print over a white or colored underbase for maximum pop on darks.” A white base is brightest; a base close to the glitter’s color makes the flake look denser. The metallic spec doesn’t call for an underbase, but many printers use a flashed one on darks to brighten the metal. Sample both ways.
Why is my glitter ink clogging the screen?
Usually the mesh is too fine for the flake. Champion’s glitter spec calls for 25–40 mesh because “glitter flake needs a large opening.” Other causes: ink that wasn’t stirred, so the flake load is uneven; a fast stroke or light flood instead of a “slow stroke, firm flood”; and flash heat gelling ink in the screen. Stir well and keep flash heat off the screen.
What is the difference between shimmer and metallic ink?
Shimmer carries fine pearlescent pigment for a soft pearl glow; Champion describes “smooth shimmer without coarse flake” that “Prints like regular plastisol” on 110–156 mesh. Metallic carries fine metallic flake for a brighter, mirror-like sheen and needs a more open 86–125 mesh. Metallic should also be printed last in the sequence, so nothing covers the flake.
Can you print over metallic ink?
Avoid it. Champion’s metallic spec says to “Print last in the sequence and avoid printing over it wet,” since anything on top hides the flake. The one exception it names is finishing: “a hot press or a clear top-coat adds extra shine.” If you top-coat, flash the metallic first, then print a clear such as Overprint Clear Gel over it.