Guide
Plastisol Ink Additives & Reducers: What Each One Does
Champion Inks

Each plastisol ink additive solves a specific problem. A curable reducer thins the ink and softens the hand. A quick flash reducer shortens flash times between layers. A soft hand base is a base you print alone or tint into soft-hand colors. An extender base makes colors more transparent and softer, and makes the ink go further. Stretch and puff additives add elasticity or a raised, 3D finish. Weigh every addition against the ink, stay inside the label's range, and test-print before the run.
Rule one: weigh it, test it, don't over-reduce
Additives work in measured amounts. Most of Champion's additive labels give their ratios as a percentage by weight, so use a scale, not a stir stick and a guess. To add 3% to 1,000 g of ink, weigh in 30 g.
- Start at the low end of the label range, and mix until the additive is fully blended.
- Test-print on the real garment. Champion's reducer labels call for a test print before production.
- Change one thing at a time. If you need both flow and stretch, dial in one, test, then add the other, so you know which change did what.
- Log the ratio on the job ticket so the reorder prints the same.
- Cure fully and wash-test. No additive excuses an undercured ink film.
The hard limit is reduction. Champion's All Purpose and High Opacity labels say: "Do not add more than 5% reducer; over-reducing lowers opacity." Reducer thins the ink, so every stroke carries less pigment and coverage drops. Where a base ink's label sets a limit like that, count every reducer you add toward it.
Champion plastisol ink additives at a glance
Mix ratios below are quoted from each product's label, checked November 24, 2026. Follow the label on the container in hand.
| Additive | What it does | Label ratio |
|---|---|---|
| Curable Ink Reducer Soft-Flow | Lowers viscosity, smooths flow, softens the hand | 1–5% by weight |
| Quick Flash Reducer | Shortens flash times and improves flow; tuned for BR and GP series | Up to 5% by weight |
| Soft Hand Plastisol Base | A soft-hand base, printed alone or tinted with pigments | Tint to the shade you need |
| Extender Base | Adds transparency, softens the hand, improves stretch, extends ink | Up to about 50% by weight |
| Super Stretch Additive | Adds elasticity for Lycra, spandex and athletic fabrics | 15% by weight |
| Badass Puff Additive | Makes ink rise in the dryer, from subtle to extreme | 10–30% |
| Super Puff Additive | Raised 3D effect with a soft, matte finish | 10–20% by weight |
Curable Ink Reducer Soft-Flow
Reach for it when the ink is too stiff to print cleanly: fine lines, halftones, large flood areas or a soft-hand fashion print. Champion's label describes a modifier "engineered to reduce viscosity, improve printability, and enhance softness," and says it "Maintains full cure performance at 320°F–330°F (160°C–165°C)."
- Ratio: 1–5% by weight, adjusted for the viscosity you want.
- Method: mix until fully incorporated, then test-print to check viscosity and coverage before full production.
- Cure: cure as normal. The label says the reducer works with all plastisol inks, including low-cure and specialty systems. It gives no separate low-cure figure, so cure to the base ink's label and confirm with a wash test.
Quick Flash Reducer
When the flash is the slowest station on a multi-layer print, this is the additive to test. Champion's label says it is "engineered to reduce flash times, improve ink flow, and enhance print smoothness." It is "Specially optimized for BR and GP series plastisol inks," and the label says it also works with other plastisols.
- Ratio: up to 5% by weight of ink.
- Best for: underbases and multi-layer prints on cotton and cotton/poly blends.
- Watch: the label says it preserves opacity and adhesion "when used correctly." Test-print, adjust, and count it toward any reducer limit on the base ink.
Soft Hand Plastisol Base
Soft Hand Base is not a reducer. It is a phthalate-free base that you print on its own or tint with pigments to build custom colors with a soft, retail-style hand on cotton, blends and synthetics. Champion's label says it keeps "excellent opacity," which is what separates it from an extender.
- Cure: "Heat-cure at 320°F (160°C) for 2–3 minutes." The label adds: "This product does not air dry."
- Mesh: up to 355 for fine detail; drop to a lower mesh for higher opacity.
- Thinning it: the label keeps minor viscosity adjustments to about 5% by weight and allows heavier reduction only "when opacity is not critical." Ask Champion which reducer to pair with the base before you thin it.
- Storage: below 90°F (32°C), in a cool, dry place.
Extender Base
Extender Base goes into your existing plastisol colors. Champion's label lists four jobs for it: it "lightens color strength, softens hand, improves stretch, and extends ink volume while maintaining adhesion and wash fastness on cotton and blends." Use it for semi-transparent tints, tone-down effects and softer prints.
- Ratio: add as needed, "up to ~50% by weight for semi-transparent effects," increasing gradually while you test-print.
- Opacity: it is transparent and lowers the opacity of the mixed ink. Keep it out of underbase whites, where you need every bit of coverage.
- Cure: the entire ink layer must reach 320–330°F.
- Polyester: on light polyester, the label says to always test for dye migration before production.
Super Stretch Additive
Standard plastisol printed on Lycra, spandex or compression fabric can crack when the garment stretches. Champion's Super Stretch Additive "transforms standard plastisol inks into high-performance stretch systems ideal for Lycra, Spandex, and athletic fabrics."
- Ratio: "Blend 15% Super Stretch Additive by weight into plastisol ink for maximum elasticity."
- Compatible inks: the label lists Champion's PFGP (General Purpose, 100% cotton), PFBR (cotton and polyester blends) and PFAP (cotton, polyester, Lycra and spandex) systems.
- Mesh: 110–230.
- Cure: the additive goes into a plastisol ink, so the entire ink film still has to reach that ink's full cure temperature. Stretch-test and wash-test a sample before the run.
Printing a lot of performance wear? A ready-made stretch ink can be simpler than modifying every color. See Champion's stretch plastisol inks for polyester and athletic fabrics and our stretch plastisol printing guide.
Puff additives: Badass Puff and Super Puff
Both turn regular plastisol into a puff ink that rises in the dryer. They differ in range and finish:
- Badass Puff Additive: blend 10–30% into plastisol ink, from the low end for subtle texture to the high end for an extreme rise. Print through 86–110 mesh, flash at 220°F for 3–5 seconds, and give it a final cure of 320–330°F "for full puff activation."
- Super Puff Additive: blend 10–20% by weight "to control puff height," for a soft, matte finish. Print through 60–110 mesh for heavier deposits and maximum puff. Its label lists the same PFGP, PFBR and PFAP systems as compatible.
Puff needs mass: an open mesh, a thick stencil and bold artwork, because large shapes rise better than hairlines. Flash lightly. Champion's Puff label gives the fix when ink starts rising early: "If it puffs at the flash, lower the flash temperature or raise the flash height." For puff in ready-mixed colors, White included, see the puff plastisol inks.
Water-based and solvent inks use different additives
Additives are made for one ink chemistry. Keep plastisol modifiers in plastisol, water-based additives in water-based ink, and solvent thinners in the ink series they are labeled for.
Water-based ink dries as its water evaporates, and a retarder slows that down in the screen. Champion's Water-Based Ink Retarder is made to keep the ink workable longer: "Add approximately 1–2% by weight directly into the ink to fine-tune open time based on shop conditions." Don't overdo it; the label warns, "Using too much retarder can slow cure and affect print durability." For heat-sensitive fabrics, the OPTI-Drive Low Cure Additive lowers the curing temperature of water-based ink. Add only what you need for immediate use, because its label gives mixed ink a 24-hour shelf life. See the full water-based ink range.
Solvent inks are thinned and slowed with solvents matched to each ink series. Champion names the series in each product title: the OPTI-971 Slow Thinner is for the 10000 Series and the OPTI-920 Slow Thinner for the 40000 Series, for example. Choose the thinner or retarder labeled for your series from the solvent ink reducers and retarders.
Shop the inks
Find the curable and quick flash reducers and the soft hand and extender bases in Champion's plastisol reducers and bases, and the stretch and puff agents in the performance additives for stretch and puff. Not sure which one your job needs? Tell us the ink, the fabric and the effect you're after.
Frequently asked questions
What does a curable reducer do in plastisol ink?
A curable reducer lowers the ink's viscosity so it flows through the mesh more easily, and it softens the hand of the print. It is formulated to cure with the ink, so the print still needs a full cure. Champion's Curable Ink Reducer Soft-Flow goes in at 1–5% by weight; test-print, then cure to the base ink's label.
How much reducer can I add to plastisol ink?
Follow both labels: the reducer's and the ink's. Champion's Curable Ink Reducer Soft-Flow runs 1–5% by weight, and the Quick Flash Reducer up to 5% by weight of ink. Champion's All Purpose and High Opacity labels cap reducer at 5% and warn that over-reducing lowers opacity, so count every reducer you add toward that limit.
What is the difference between soft hand base and extender base?
Soft hand base is a base you print alone or tint with pigments to make custom soft-hand colors; Champion's label says it keeps excellent opacity. Extender base goes into existing colors to make them more transparent and softer, improve stretch and extend the ink, at up to about 50% by weight for semi-transparent effects. Both need a full heat cure.
Will adding reducer lower opacity?
It can, and the more you add, the more it does. Reducer thins the ink, so each stroke carries less pigment. Champion's All Purpose and High Opacity labels put it plainly: over-reducing lowers opacity. Keep reductions small, test-print on the actual garment, and don't thin an underbase white to fix a coverage problem.
How do I make plastisol ink stretch more?
Add a stretch additive or switch to a stretch ink. Champion's Super Stretch Additive goes in at 15% by weight for Lycra, spandex and athletic fabrics, and its label lists the PFGP, PFBR and PFAP systems as compatible. For regular performance work, a ready-made stretch plastisol can be simpler. Either way, verify the cure: an undercured print cracks when stretched.