Guide
Plastisol Ink: The Complete Guide for Screen Printers
Champion Inks

Plastisol ink is a heat-cured screen printing ink made of PVC resin particles suspended in a liquid plasticizer, plus pigment. It never air-dries: it stays workable in the screen until heat fuses it into a flexible, opaque film, and the whole ink film has to reach the cure temperature listed for that ink. Choose the series by fabric, print it through the mesh its specs call for, gel it at the flash and cure it fully in the dryer.
Every temperature, mesh range and limit below is quoted from the Champion product page it belongs to. If the label on your container disagrees with any chart, including this one, follow the label. More how-to guides live in the Champion Learning Center.
What plastisol ink is (and why it never air-dries)
Champion’s own definition is a good place to start: “Plastisol—a suspension of PVC particles in plasticizer—remains an industry standard for opacity, vibrant color, durability, and workable print windows.” There is no water or solvent in the ink to evaporate, so plastisol can sit in an open screen through a long run without drying in the mesh. Champion’s Soft Hand Base page says it plainly: “This product does not air dry.”
Heat is what changes it. As the ink warms, the PVC particles start to absorb the plasticizer and swell, and the ink gels: the surface turns dry to the touch, but the film is still weak. Keep heating and the particles fuse into a tough, stretchy film that grips the fabric. That second stage is the cure, and it has to happen through the whole deposit, top to bottom. The All Purpose page lists its cure as “320°F (160°C) – entire ink film must reach temperature.”
Water-based ink works the other way. It dries as the water leaves, so it can dry in the screen during a run, and Champion’s water-based textile page says to cure “only after all moisture has driven off.” The payoff is hand: the same page describes “a breathable, lightweight print that feels integrated into the fabric.” Plastisol sits on top of the fabric as a film, which is where its strong coverage on dark garments comes from. Champion also stocks water-based textile inks.
Choose the series by fabric
Fabric decides more than anything else. Cotton takes standard-cure ink without trouble; polyester brings dye migration (garment dye bleeding into the ink when it is heated) and heat sensitivity; nylon needs extra adhesion. Here is how Champion’s plastisol line maps to fabric, or you can find the right ink for your fabric with the ink finder.
| Fabric | Champion series | What the product page says |
|---|---|---|
| 100% cotton | General Purpose; High Opacity | General Purpose: “bright, long-lasting prints on cotton and blended fabrics.” High Opacity: “bold, bright prints on dark cotton with fewer strokes.” |
| Cotton/poly blends | All Purpose; Bleed Resistant | All Purpose: “prints cleanly on 100% cotton, 50/50 and tri-blends, and light polyester.” Bleed Resistant: “High-opacity bleed control,” for 50/50 blends and light-colored polyester. |
| 100% polyester and athletic wear | Athletic Polyester; Extreme 270° Low Cure; Sport; Stretch | Athletic Polyester: “high-opacity, low-bleed, low-cure.” Extreme 270°: “a cure temperature as low as 270°F (132°C).” Sport: built for “polyester, spandex, and moisture-wicking performance wear.” |
| Nylon and coated fabrics | Nylon White (catalyst required for nylon) | “formulated for nylon, polyester, coated fabrics, and blends.” |
100% cotton
Cotton is the forgiving fabric. It doesn’t carry the dye-migration risk that polyester does, so standard-cure inks work well. For everyday cotton work, General Purpose Plastisol Ink lists “Short Flash Times” and a cure range of 320–330°F (160–165°C). For dark shirts where you want coverage in fewer strokes, High Opacity Plastisol Ink has a “Low tack” body that “reduces lift-off between colors for faster wet-on-wet production.”
Cotton/poly blends and tri-blends
The polyester in a blend is colored with dyes that can move into the ink when it is heated, which is how a white print on a red shirt turns pink. All Purpose Plastisol Ink is the one-series answer for mixed work, with a “Low-bleed formula – resists dye migration on cotton/poly blends.” When the blend is darker or higher in polyester, step up to bleed-resistant plastisol; for dark polyester, the Bleed Resistant page recommends “a white blocker underbase (e.g., 5-Star Bright White).” Either way, test-print the actual blank first.
100% polyester and athletic wear
Polyester asks for two things at once: bleed resistance and less heat. Athletic Polyester Plastisol Ink covers both, with a “Low cure (280–300°F)” that “protects sensitive fabrics from scorching or shrinkage.” The Extreme 270° low-cure series goes lower still: “270°F–290°F (132°C–143°C) for full cure.”
Sport plastisol and Stretch plastisol are built for movement. Sport lists 100% polyester, including sublimated fabrics, among its substrates but cures at a standard 320°F–330°F, so test dye-sensitive garments carefully. Stretch is a “high-elasticity plastisol” for sportswear, activewear and swimwear.
Nylon and coated fabrics
Nylon jackets, bags and coated fabrics are about adhesion. Nylon White Plastisol Ink is a bleed-resistant white whose product page marks the catalyst as “Required for Nylon”: “Add 15–20% by weight to the ink.” Mix only what the job needs, because “Pot life is limited once catalyzed; unused mixed ink will harden.” Contact Champion about the catalyst before a nylon job.
Whites, underbases and blockers
White does the heavy lifting in most shops, as the underbase on dark garments and as the top white. Champion’s white plastisol inks are split by fabric, from General Purpose White for cotton to Extreme 270° White and Athletic White for polyester. On dye-prone polyester, a gray blocker underbase goes down first; IronBlock LC lists its top coats as “Compatible with white or color plastisol inks.” For technique, follow the step-by-step white plastisol printing guide.
Mesh and squeegee basics
Mesh count is one of the biggest controls on how much ink reaches the shirt. Lower counts have larger openings and lay down a heavier, more opaque deposit; higher counts lay down less ink, hold finer detail and feel softer. Champion’s core plastisol pages start in the same place: All Purpose calls for “110–160 for solids; 200–230 for detail and halftones,” and General Purpose for “110–160 for standard prints; 200+ for fine detail.” All Purpose pairs that with a “65–75 durometer, medium pressure” squeegee.
Specialty inks break the pattern. Glitter needs an “Open mesh: 25–40” so the flake can pass through, while Four Color Process Plastisol Ink runs “230–305 (higher mesh for finer line counts).” Check the specs for the ink you are burning a screen for.
Flash vs full cure
A flash unit and a dryer do different jobs. The flash only gels a layer so the next screen can print on top without lifting or smearing it; All Purpose lists “220–250°F (104–121°C), 3–5 sec – until surface is dry to the touch.” Stop at dry to the touch. Champion’s white plastisol guide warns that over-flashing “can cause ink stacking, rough texture, or dye bleed on sensitive fabrics.”
The full cure happens in the dryer, and the target depends on the series: Champion lists 320°F (160°C) for All Purpose, 320–330°F (160–165°C) for General Purpose, 280–300°F for Athletic Polyester and 270°F–290°F (132°C–143°C) for Extreme 270° Low Cure. Measure the ink film itself, with temperature strips or a probe on the print, rather than trusting the dryer’s setpoint. If prints crack when stretched or fade in the wash, suspect undercure first.
Color work: spot colors, custom color matching and CMYK
Spot color is where plastisol shines: each color is mixed to a target and printed through its own screen. Champion mixes custom colors to order in its plastisol series: send your color code through the CHAMP-MIX™ Custom Color Match page. For in-house mixing, CHAMP-MIX™ Mixing White is labeled “semi-transparent – use a white underbase on dark fabrics.” Choose the color from a physical color guide, not a screen, as the Custom Color Match listing advises: “Do not pick a color off your monitor.” Then approve the cured print against that guide.
For photographic art on light garments, four color process plastisol is “a phthalate-free, semi-transparent CMYK system matched to process standards for photorealistic halftone printing on light garments.”
Modifying plastisol: reducers, bases and additives
Most plastisol is made to print straight from the pail; High Opacity says to “use straight from the container; stir before use.” Stir first, because ink that looks stiff in the bucket loosens once it is worked. If you still need to thin it, stay inside the limit on the All Purpose and High Opacity pages: “Do not add more than 5% reducer; over-reducing lowers opacity.”
- Curable Ink Reducer thins ink for smoother flow and a softer hand at “1–5% by weight (adjust for desired viscosity).”
- Quick Flash Reducer is made to shorten flash times and is “Specially optimized for BR and GP series plastisol inks”; add “up to 5% Quick Flash Reducer by weight.”
- Extender Base “Reduces opacity for transparent/tone-down effects and softer prints.”
- Super Stretch Additive: “Blend 15% Super Stretch Additive by weight into plastisol ink for maximum elasticity.”
Weigh additions, mix thoroughly, make a test print and re-check the cure, because anything that changes the ink can change how it prints and cures. Browse plastisol reducers and additives.
Plastisol transfers in brief
Plastisol can also be printed onto transfer paper and heat-pressed later. The Transfer Plastisol Ink page lists the steps: print mirrored, flash, gel, dust with transfer adhesive powder and let it set before the final gel, then “Press at 315°F–350°F (157°C–177°C) for 10–15 seconds under medium to high pressure.” Stop at a gel before pressing; the Transfer White page says, “Avoid full cure pre-press; aim for gel so transfer bonds properly.”
Storage, shelf life and handling
The All Purpose page says: “Store at 65–90°F (18–32°C), away from direct sun and heat. Keep the lid sealed.” It lists a shelf life of “12 months in a sealed container.”
- Rotate stock. Date each container when it arrives, use the oldest first and close lids between pulls.
- Stir before use. Specialty inks need it most: the Glitter page notes that “glitter settles,” and the Metallic page that “metallic flake settles.”
- Mind the temperature. Cold ink stiffens, so let it warm to shop temperature and stir before reaching for reducer. Ink stored hot can start to thicken in the container.
Safety and compliance
The All Purpose page states: “Phthalate-free formulation, made to meet CPSIA lead and phthalate limits for children’s products.” That is a statement about the ink, not the finished garment. The U.S. Consumer Product Safety Commission says a decorator may be able to rely on an ink supplier’s component testing under 16 CFR part 1109, “but you must still issue a CPC for the finished product” (CPSC’s Children’s Product Certificate example for clothing).
For handling, the same page says: “Wear gloves and eye protection; use with adequate ventilation.” Champion’s series Safety Data Sheets cover every color in the series. If you need a sheet or documentation for a customer, ask Champion for an SDS or technical help.
Shop the inks
- Shop Champion plastisol inks, every series in one place.
- White plastisol inks for underbases and top whites.
- Extreme 270° low-cure plastisol for heat-sensitive polyester.
- CHAMP-MIX™ Custom Color Match for brand colors.
- Still deciding? Use the ink finder.
Specifications on this page are quoted from Champion’s product pages on championinks.com, last reviewed November 24, 2026. Specs can change; if the label on the container you are printing differs, follow the label.
Frequently asked questions
What is plastisol ink made of?
PVC resin particles suspended in a liquid plasticizer, plus pigments and additives. Champion describes it as “a suspension of PVC particles in plasticizer.” With no water or solvent to evaporate, it stays wet until heat fuses it into a flexible film.
Does plastisol ink dry on its own?
No. Plastisol does not air-dry, so it can sit in an open screen through a long run. It gels at the flash and cures only when the whole ink film reaches its full-cure temperature.
What temperature does plastisol ink cure at?
It depends on the series: Champion lists 270°F–290°F (132°C–143°C) for Extreme 270° Low Cure, 280–300°F for Athletic Polyester, 320°F (160°C) for All Purpose and 320–330°F (160–165°C) for General Purpose. The entire ink film has to reach it.
How long does plastisol ink last?
Champion’s All Purpose page lists a shelf life of 12 months in a sealed container, stored at 65–90°F (18–32°C) away from direct sun and heat. Use the oldest stock first and stir before use.
Is plastisol ink phthalate-free?
Not automatically; formulas vary by manufacturer, so check the product information and Safety Data Sheet. Champion’s All Purpose page states a “Phthalate-free formulation, made to meet CPSIA lead and phthalate limits for children’s products,” as do other Champion series. Finished children’s products still need their own Children’s Product Certificate.