Guide
Solvent & UV Screen Printing Ink for Plastic, Metal, Signs
Champion Inks

Solvent screen printing ink is chosen by substrate. The ink has to bite into the surface you're printing, so a series made for vacuum-formed plastics won't necessarily hold on vinyl or polyethylene. Pick the Champion Inks® series whose label names your material, dry it the way that label says, and prove adhesion on the real part before the run. UV-curable inks follow the same rule with one difference: they cure under UV light instead of drying by evaporation.
Champion specs below are quoted from each product's page as published on November 24, 2026. Drying temperatures are given in °F, as printed on the labels.
Choose solvent screen printing ink by substrate
| You're printing | Champion series | From the label |
|---|---|---|
| Vacuum-formed plastics: ABS, acrylic, polystyrene, polycarbonate, COP | 10000 Series Multi-Vac ink for plastics | Solvent-based ink with a scuff-resistant gloss finish |
| Metal, glass, treated polyethylene and polypropylene, PC boards | 20000 Series two-part epoxy | Mixed with a catalyst; built for industrial and electronic work |
| HDPE, LDPE, treated polyethylene, cardboard, wood, metal | 30000 Series industrial topcoat | Air dries, jet dries or bakes for enhanced hardness |
| Flexible vinyl, rigid PVC, pressure-sensitive decals, coated polyester | 40000 Series gloss vinyl ink or 43000 Series matte vinyl ink | Same substrates; choose a high-gloss or a low-glare matte finish |
| Polyurethane, nylon, polyester, leather, rubber, canvas | 66000 Series polyurethane ink | Flexible air-dry ink rated 55D |
| Treated and untreated polyester, PET, PET-G, nylon, coated metal | 76000 Series polyester ink | Air-dry ink with a glossy, scuff-resistant finish |
| Corrugated plastic (Coroplast), polypropylene, polyethylene | 80000 Series Coroplast ink | Air dries with no heat; made for yard signs and outdoor signage |
Overlaps are normal. Nylon appears on both the 66000 and 76000 labels, and polyethylene on the 20000, 30000 and 80000 labels. When two series list your material, choose by what the part has to survive: the 66000 label stresses flexibility (“Rated 55D for elasticity without cracking or peeling”), the 20000 label abrasion and chemical resistance, and the 80000 label outdoor sign work. Then let an adhesion test make the final call.
Screen printing on metal? The 20000 label lists metal and glass, the 30000 label lists metal along with glass and coated metal, and the 76000 label lists coated metal. A painted or coated part prints like its coating, not the metal underneath, so test on a finished part.
Air dry, jet dry, bake: reading the label
| Series | Air dry | Jet dry (forced hot air) | Bake | Mesh |
|---|---|---|---|---|
| 10000 | About 30 minutes | 20–30 seconds at 135°F–180°F | Not listed | 230–280 |
| 20000 (two-part) | 30 minutes | 20–30 seconds at 135–180°F | Not listed | 230–280 |
| 30000 | 20–30 minutes | 40–60 seconds at 150–180°F | 350°F for 8–9 minutes, for enhanced hardness | 230–280 |
| 40000 | 20–30 minutes | 40–60 seconds at 150–180°F | Not listed | 230–280 |
| 43000 | 20–30 minutes | 40–60 seconds at 150°F–180°F | Not listed | 230–280 |
| 66000 | 30 minutes | 20–30 seconds at 135–180°F | Not listed | 230–280 |
| 76000 | 30 minutes | 20–30 seconds at 135–180°F | Not listed | 230–280 |
| 80000 | 30–60 minutes; forced air speeds it up | No figure given | Not listed | 200–305 for fine detail; 110–160 for bold prints |
How to read it:
- Air dry means the solvent evaporates at room temperature. Rack prints with space for air to move; a cold shop or a heavy deposit takes longer.
- Jet dry means forced hot air at the label's time and temperature; watch thin or heat-sensitive plastics for distortion.
- Dry isn't ready to stack. Before you box a run, stack a few test pieces and check they don't stick together.
- Stencil and mesh. Use a solvent-resistant stencil: most labels name a dual-cure or SBQ emulsion, and the 80000 label allows emulsion or film. Every series except the 80000 lists 230–280 mesh; the 80000 label gives 200–305 for fine detail and 110–160 for bold prints.
Two-part epoxy: catalyst handling
The 20000 Series Epoxy is a “two-part epoxy screen printing ink system designed for industrial and electronic applications.” Its label says it “Activates with a catalyst for exceptional hardness and resistance,” and sets three rules:
- “Combine ink with catalyst per manufacturer instructions prior to printing.”
- “Avoid mineral spirits, as they can freeze the ink.”
- “Verify adhesion and resistance before full production.”
The catalyst is listed as its own option on the 20000 Series quart. The label doesn't give a numeric mix ratio or a pot life, so get both from Champion before the job: ask Champion about your substrate and the catalyst. Then, as with any catalyzed ink:
- Measure both parts to Champion's ratio and mix thoroughly. Mix only what you can print within the pot life, and write the mix time on the container.
- Clean screens, squeegees and tools before mixed ink sets in the mesh.
- A two-part ink keeps curing after the solvent has gone, so run adhesion and chemical-resistance tests after the cure time Champion gives you, not straight off the rack.
Thinners, retarders and wash-ups
- Thinner (reducer) lowers viscosity so the ink flows and prints cleanly. Fast thinners evaporate quickly; slow thinners keep the ink open longer.
- Retarder slows evaporation so ink doesn't dry in the screen, which helps in hot shops, on long runs and on fine detail.
- Wash-up cleans screens, squeegees and tools. It isn't an ink additive unless its label says it doubles as one, as the OPTI-900 label does: it “Acts as both a fast-drying thinner and an effective wash-up solvent.”
Champion's labels give additions by weight: the Multi-Vac 10000 label lists T-971 thinner at 5–15%, and the OPTI-971 Slow Thinner page, “Designed for 10000 Series Screen Inks,” gives the same range. OPTI-999 Super Retarder is “engineered to extend drying time, improve ink flow, and boost adhesion on non-porous plastics.”
Each OPTI thinner, retarder and wash-up below names its series in the product title:
| Series | OPTI products named for it |
|---|---|
| 10000 | OPTI-938 Fast Thinner, OPTI-971 Slow Thinner, OPTI-925 Mild Lacquer Wash-Up |
| 20000 | OPTI-976B reducer for industrial two-part inks |
| 40000 | OPTI-912 Fast Thinner, OPTI-920 Slow Thinner, OPTI-934B Retarder, OPTI-911 Wash-Up Thinner |
| 66000 | OPTI-974 Slow Thinner / Retarder, OPTI-922 Biting & Retarder |
| 76000 | OPTI-631 Retarder, OPTI-637 Wash-Up |
| 80000 | OPTI-900 Fast Thinner / Wash-Up, OPTI-910 Slow Thinner |
The rule: use what your series label calls for, at the percentage it gives, and choose OPTI products that name your series. If your series isn't in the table, or you can't match a product your label names, ask Champion before you mix: the wrong solvent can ruin a batch. The full line is under OPTI thinners, retarders and wash-ups.
Test adhesion on the real substrate
Most Champion solvent labels say to pre-test, as the 43000 label does: “Always test on actual substrate before production to confirm adhesion and durability.” A routine that holds up:
- Use real parts from the production lot, cleaned of dust, oil and mold release with a cleaner your substrate supplier approves.
- Print the production setup: same mesh, stencil, ink and additions.
- Dry or cure exactly as you will in production, and wait the full time before testing.
- Run a cross-hatch tape test. Score a small grid through the ink to the substrate with a sharp blade, press a strong pressure-sensitive tape over it, pull it off sharply and look at how much ink lifts. The method is standardized in ASTM D3359.
- Add the tests the part will face: flexing for flexible materials (the 66000 label asks you to verify “adhesion and flexibility”), rubbing with the chemicals or cleaners it will meet, and outdoor exposure for signs.
- Write it down: substrate lot, ink and additions, drying settings and results.
Polyethylene and polypropylene need extra care. These low-surface-energy plastics are usually treated (corona, flame or plasma) so ink can wet and grip them. Champion's labels list treated grades for the 20000 and 30000 series, and the OPTI-900 label refers to “corona-treated polyethylene/polypropylene.” Treatment can fade with time and storage, so ask your supplier which side is treated, check older stock with dyne test pens, and test each new lot.
UV-curable screen inks: what to know
UV-curable inks don't dry by evaporation. They cure when UV light triggers a reaction in the ink film, so they stay workable in the screen until they meet a UV source; keep them out of direct daylight. A full cure comes down to a few controls:
- Dose and intensity. Cure depends on how much UV energy reaches the ink (dose) and how strong it is at the surface (intensity). Lamp power, lamp age, reflector condition and distance change both; belt speed changes the dose. A UV radiometer measures what actually reaches the part.
- Lamp match. LED lamps emit a narrow band of UV and mercury lamps a broad spectrum, so use an ink formulated for your lamp type.
- Deposit. Opaque whites, dark colors and heavy deposits are harder to cure all the way through. Print the thinnest deposit that covers.
- Verification. Under-cured prints show up as tackiness, poor adhesion, sticking in stacks and odor; check with the tape test above and a solvent-rub test. Over-curing can cause brittleness or poor adhesion of the next layer.
Champion's UV DTF label says the same: “Confirm lamp health and irradiance; insufficient UV can reduce adhesion and mar resistance.” Uncured UV ink can irritate or sensitize skin, so wear gloves and read the SDS. Before you commit to a UV-curable screen ink, talk to Champion about your substrate and your lamps.
Custom colors for solvent series
Champion's Solvent Custom Color Match is listed with seven series: Solvent 10000, 20000, 30000, 40000, 43000, 66000 and 80000. Order the match in the same series you'll print, so the color arrives in the chemistry that sticks to your substrate. The 76000 isn't on that list, so ask Champion first if you print it. See Solvent Custom Color Match, or send your color code through CHAMP-MIX™ Custom Color Match.
Safety: ventilation, PPE and SDS
- Ventilate. The 80000 label: “Operate in a well-ventilated area or use fume extraction.”
- Wear the gear. The 80000 label lists “Gloves, eye protection, and respirator as needed”; the 20000 label adds protective clothing, and the 66000 label specifies solvent-resistant clothing.
- Read the SDS first. The 20000 and 40000 labels put it plainly: “Review the Safety Data Sheet before use.” Champion publishes series sheets that cover every color in a series; check yours for flammability, storage and respirator guidance.
- Handle solvents like solvents. Keep containers closed, keep ignition sources away from the print and drying area, and store solvent-soaked rags in a closed metal container. Store ink away from heat and sunlight; the 20000 label gives 65–90°F.
Not sure a series will hold on your part, or can't find its sheet? Contact Champion before you buy.
Shop the inks
- 80000 Series ink for Coroplast yard signs
- Solvent thinners, retarders and wash-ups
- Custom-matched solvent colors
Or browse every series in Champion solvent and UV inks, and find more print guides in the Champion Learning Center.
Frequently asked questions
What kind of ink do you use to screen print on plastic?
A solvent or UV ink made for that plastic. Champion's 10000 Series Multi-Vac covers vacuum-formed ABS, acrylic, polystyrene, polycarbonate and COP; the 80000 Series corrugated plastic, polypropylene and polyethylene; the 76000 PET and PET-G; and the 40000 and 43000 vinyl and PVC. Polyethylene and polypropylene usually need surface treatment. Always test adhesion on the actual part.
What ink works on Coroplast yard signs?
Use an air-dry solvent ink made for corrugated plastic. Champion's 80000 Series is labeled for Coroplast, polypropylene and polyethylene, air dries in 30–60 minutes with no heat (forced air speeds it up), and lists 110–160 mesh for bold prints or 200–305 for fine detail. Use sign stock treated for printing, and tape-test before the full order.
What is the difference between a thinner and a retarder?
A thinner lowers the ink's viscosity so it flows and prints cleanly; fast and slow thinners also change how quickly it dries. A retarder's main job is to slow evaporation, so ink stays open in the screen during long runs, fine detail or hot conditions. Use the ones your series label names, by weight, within its percentage range.
Do solvent inks need heat to cure?
Not usually. Champion's air-dry series dry by solvent evaporation at room temperature, in 20 to 60 minutes depending on the series. Heat speeds things up: the labels give jet-dry times at 135–180°F or 150–180°F, and the 30000 Series can be baked at 350°F for enhanced hardness. Two-part inks like the 20000 epoxy also need their catalyst to reach full hardness.
How do you test ink adhesion on plastic or metal?
Print real parts with your production setup and let them dry or cure fully. Then run a cross-hatch tape test: score a small grid through the ink, press strong tape over it, pull it off sharply and check how much ink lifts. Add the stresses the part will face, such as flexing, chemical rubs or outdoor exposure, and record the results.